General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 - 8.92 g/cm³ Show Material materials with Densidad of 8.9 - 8.92 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Dureza Vickers | 20.0 °C | 110 [-] Show Material materials with Dureza Vickers of 110 [-] | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 20.0 °C | 127 GPa Show Material materials with Módulo elástico of 127 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 386 J/(kg·K) Show Material materials with Calor específico of 386 J/(kg·K) | |
100.0 °C | 395 J/(kg·K) Show Material materials with Calor específico of 395 J/(kg·K) | ||
200.0 °C | 407 J/(kg·K) Show Material materials with Calor específico of 407 J/(kg·K) | ||
Coeficiente de dilatación térmica | 300.0 °C | 1.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K | |
Conductividad térmica | 20.0 °C | 350 W/(m·K) Show Material materials with Conductividad térmica of 350 W/(m·K) | |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.80E+7 S/m Show Material materials with Conductividad eléctrica of 4.80E+7 S/m |
Specific Electrical conductivity | 83 % IACS Show Material materials with Specific Electrical conductivity of 83 % IACS |
Chemical properties