CuNi9Sn2 (CW351H) is comparable to CuNi9Sn2, mat. no. 2.0875, acc. to DIN 17664 : 1983-12. To the comparable DIN-mark applies: The material shows high strength specific values as well as favorable tarnish-proofness and a very good stress relaxation behaviour in spring-hard condition. CuNi9Sn2 has sufficient electrical and thermal conductivity. Favorable corrosion resistance in natural resp. industrial atmosphere. Also resistance to different waters, humidity, non-oxidizing acids, bases and saline solutions. No risk of stress corrosion. Processing properties: warm forming: good cold forming: very good machinability: unfavorable hard soldering: very good soft soldering: very good gas-shielded welding: very good burnishing: very good Application: For elastic components in relay, pushbutton switchers, connectors and receptacles in communications engineering, in EDP-systems, in consumer electronics equipment and in automobile electronics, for switcher components, soldering tags and frames, boxes for electrical components, carrier plates for integrated circuits an for conductor board pens. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.89 - 8.9 g/cm³

Show Material materials with Densidad of 8.89 - 8.9 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Elongación

20.0 °C

40 %

Show Material materials with Elongación of 40 %

Elongación A50

20.0 °C

30 %

Show Material materials with Elongación A50 of 30 %

Límite elástico Rp 0,2

20.0 °C

250 MPa

Show Material materials with Límite elástico Rp 0,2 of 250 MPa

Módulo elástico

20.0 °C

140 GPa

Show Material materials with Módulo elástico of 140 GPa

Resistencia a la tracción

20.0 °C

340 - 410 MPa

Show Material materials with Resistencia a la tracción of 340 - 410 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

370 J/(kg·K)

Show Material materials with Calor específico of 370 J/(kg·K)

100.0 °C

390 J/(kg·K)

Show Material materials with Calor específico of 390 J/(kg·K)

200.0 °C

410 J/(kg·K)

Show Material materials with Calor específico of 410 J/(kg·K)

Coeficiente de dilatación térmica

100.0 °C

1.55E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.55E-5 1/K

200.0 °C

1.59E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.59E-5 1/K

300.0 °C

1.66E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.66E-5 1/K

Unlock all property charts

Conductividad térmica

20.0 °C

48 W/(m·K)

Show Material materials with Conductividad térmica of 48 W/(m·K)

100.0 °C

56 W/(m·K)

Show Material materials with Conductividad térmica of 56 W/(m·K)

200.0 °C

65 W/(m·K)

Show Material materials with Conductividad térmica of 65 W/(m·K)

Unlock all property charts

Temperatura de fusión

915 - 1240 °C

Show Material materials with Temperatura de fusión of 915 - 1240 °C

Typical for Wrought Copper Nickel Grade

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

6.40E+6 S/m

Show Material materials with Conductividad eléctrica of 6.40E+6 S/m

Specific Electrical conductivity

11 % IACS

Show Material materials with Specific Electrical conductivity of 11 % IACS

Chemical properties

PropertyValue

Estaño

1.8 - 2.8 %

Show Material materials with Estaño of 1.8 - 2.8 %

Hierro

0.3 %

Show Material materials with Hierro of 0.3 %

Manganeso

0.3 %

Show Material materials with Manganeso of 0.3 %

Níquel

8.5 - 10.5 %

Show Material materials with Níquel of 8.5 - 10.5 %

Plomo

0.03 %

Show Material materials with Plomo of 0.03 %

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %