General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.85 - 8.9 g/cm³ Show Material materials with Densidad of 8.85 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Dureza Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Dureza Vickers of 75 - 105 [-] |
Elongación | 20.0 °C | 55 % Show Material materials with Elongación of 55 % |
Elongación A50 | 20.0 °C | 45 % Show Material materials with Elongación A50 of 45 % |
Límite elástico Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa |
Módulo elástico | 20.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 20.0 °C | 310 - 390 MPa Show Material materials with Resistencia a la tracción of 310 - 390 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Conductividad térmica | 20.0 °C | 96 W/(m·K) Show Material materials with Conductividad térmica of 96 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.00E+7 S/m Show Material materials with Conductividad eléctrica of 1.00E+7 S/m |
Specific Electrical conductivity | 17 % IACS Show Material materials with Specific Electrical conductivity of 17 % IACS |
Chemical properties
Property | Value |
---|---|
Estaño | 4.5 - 5.5 % Show Material materials with Estaño of 4.5 - 5.5 % |
Fósforo | 0.01 - 0.4 % Show Material materials with Fósforo of 0.01 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |