Material CuSn5, mat. No. CW451K is used in the form of tubes for manometer springs or hose tubes as well as for contact springs and connectors. Basically the same application area as CuSn6 (CW452K). CuSn5 shows slightly higher electrical conductivity at slightly lower strength due to the lower tin-content. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.85 - 8.9 g/cm³

Show Material materials with Densidad of 8.85 - 8.9 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Dureza Vickers

20.0 °C

220 [-]

Show Material materials with Dureza Vickers of 220 [-]

Módulo elástico

20.0 °C

120 GPa

Show Material materials with Módulo elástico of 120 GPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

380 J/(kg·K)

Show Material materials with Calor específico of 380 J/(kg·K)

Coeficiente de dilatación térmica

23.0 °C

1.5E-5 - 1.9E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K

Typical for Leaded Phosphor Bronze

Conductividad térmica

20.0 °C

96 W/(m·K)

Show Material materials with Conductividad térmica of 96 W/(m·K)

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

1.00E+7 S/m

Show Material materials with Conductividad eléctrica of 1.00E+7 S/m

Specific Electrical conductivity

17 % IACS

Show Material materials with Specific Electrical conductivity of 17 % IACS

Chemical properties

PropertyValue

Estaño

4.5 - 5.5 %

Show Material materials with Estaño of 4.5 - 5.5 %

Fósforo

0.01 - 0.4 %

Show Material materials with Fósforo of 0.01 - 0.4 %

Hierro

0.1 %

Show Material materials with Hierro of 0.1 %

Níquel

0.2 %

Show Material materials with Níquel of 0.2 %

Plomo

0.02 %

Show Material materials with Plomo of 0.02 %

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %