General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.79 - 8.8 g/cm³ Show Material materials with Densidad of 8.79 - 8.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Elongación | 20.0 °C | 23 - 26 % Show Material materials with Elongación of 23 - 26 % |
Elongación A50 | 20.0 °C | 20 - 23 % Show Material materials with Elongación A50 of 20 - 23 % |
Elongation A10 | 20.0 °C | 22 % Show Material materials with Elongation A10 of 22 % |
Elongation A100 | 20.0 °C | 18 % Show Material materials with Elongation A100 of 18 % |
Elongation A11.3 | 20.0 °C | 22 % Show Material materials with Elongation A11.3 of 22 % |
Límite elástico Rp 0,2 | 20.0 °C | 250 - 280 MPa Show Material materials with Límite elástico Rp 0,2 of 250 - 280 MPa |
Módulo elástico | 20.0 °C | 115 GPa Show Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 20.0 °C | 450 - 550 MPa Show Material materials with Resistencia a la tracción of 450 - 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) |
Coeficiente de dilatación térmica | 100.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K |
300.0 °C | 1.82E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.82E-5 1/K | |
400.0 °C | 1.87E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.87E-5 1/K | |
650.0 °C | 2.22E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18E-5 1/K | |
Conductividad térmica | 20.0 °C | 67 W/(m·K) Show Material materials with Conductividad térmica of 67 W/(m·K) |
200.0 °C | 81 W/(m·K) Show Material materials with Conductividad térmica of 81 W/(m·K) | |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.00E+6 - 7.50E+6 S/m Show Material materials with Conductividad eléctrica of 7.00E+6 - 7.50E+6 S/m |
200.0 °C | 6.50E+6 S/m Show Material materials with Conductividad eléctrica of 6.50E+6 S/m | |
Resistividad eléctrica | 20.0 °C | 1.33E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.33E-7 Ω·m |
200.0 °C | 1.54E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.54E-7 Ω·m | |
Specific Electrical conductivity | 12 - 13 % IACS Show Material materials with Specific Electrical conductivity of 12 - 13 % IACS |
Chemical properties
Property | Value |
---|---|
Estaño | 7.5 - 8.5 % Show Material materials with Estaño of 7.5 - 8.5 % |
Fósforo | 0.01 - 0.4 % Show Material materials with Fósforo of 0.01 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |