General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 155 - 350 [-] Show Material materials with Dureza Brinell of 155 - 350 [-] |
Dureza Vickers | 20.0 °C | 120 - 450 [-] Show Material materials with Dureza Vickers of 120 - 450 [-] |
Elongación | 20.0 °C | 2 - 15 % Show Material materials with Elongación of 2 - 15 % |
Elongación A50 | 20.0 °C | 2 - 16 % Show Material materials with Elongación A50 of 2 - 16 % |
Elongation A10 | 20.0 °C | 6 - 8 % Show Material materials with Elongation A10 of 6 - 8 % |
Elongation A100 | 20.0 °C | 5 - 10 % Show Material materials with Elongation A100 of 5 - 10 % |
Límite elástico Rp 0,2 | 20.0 °C | 450 - 1420 MPa Show Material materials with Límite elástico Rp 0,2 of 450 - 1420 MPa |
Módulo elástico | 20.0 °C | 135 GPa Show Material materials with Módulo elástico of 135 GPa |
Resistencia a la tracción | 20.0 °C | 510 - 1520 MPa Show Material materials with Resistencia a la tracción of 510 - 1520 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 300.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
Conductividad térmica | 20.0 °C | 92 - 125 W/(m·K) Show Material materials with Conductividad térmica of 92 - 125 W/(m·K) | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 8.00E+6 - 1.80E+7 S/m Show Material materials with Conductividad eléctrica of 8.00E+6 - 1.80E+7 S/m |
Specific Electrical conductivity | 23 % IACS Show Material materials with Specific Electrical conductivity of 23 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 1.8 - 2.1 % Show Material materials with Berilio of 1.8 - 2.1 % |
Cobalto | 0.3 % Show Material materials with Cobalto of 0.3 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |