Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 230 [-] Show Material materials with Dureza Vickers of 230 [-] |
Elongación | 20.0 °C | 10 % Show Material materials with Elongación of 10 % |
Elongation A100 | 20.0 °C | 6 % Show Material materials with Elongation A100 of 6 % |
Límite elástico Rp 0,2 | 20.0 °C | 760 MPa Show Material materials with Límite elástico Rp 0,2 of 760 MPa |
Resistencia a la tracción | 20.0 °C | 750 - 950 MPa Show Material materials with Resistencia a la tracción of 750 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Berilio | 0.4 - 0.7 % Show Material materials with Berilio of 0.4 - 0.7 % |
Cobalto | 0.8 - 1.3 % Show Material materials with Cobalto of 0.8 - 1.3 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.8 - 1.3 % Show Material materials with Níquel of 0.8 - 1.3 % |