Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.92 g/cm³ Show Material materials with Densidad of 8.92 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 190 [-] Show Material materials with Dureza Brinell of 190 [-] | |
Dureza Vickers | 20.0 °C | 200 [-] Show Material materials with Dureza Vickers of 200 [-] | |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % | |
Límite elástico Rp 0,2 | 20.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 20.0 °C | 650 MPa Show Material materials with Resistencia a la tracción of 650 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 385 J/(kg·K) Show Material materials with Calor específico of 385 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 1.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Fósforo | 0.15 - 0.25 % Show Material materials with Fósforo of 0.15 - 0.25 % |
Níquel | 0.8 - 1.2 % Show Material materials with Níquel of 0.8 - 1.2 % |