EN 12163 Grade CuCr1Zr R470

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

CuCr1Zr, mat. No CW106C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuCrZr, mat. No 2.1293, acc. to DIN 17666 : 1983-12 applies: The strength values of CuCrZr are more favorable than of CuCr especially at higher temperatures. CuCrZr shows the following properties: high strength at room temperature, high temperature for removal of workhardening, high creep strength, no notch sensitivity at increased temperatures. Temperature for removal of workhardening approximates 500°C. Favorable electrical and thermal conductivity. Processing properties: hot and cold forming: good machinability: moderately soft soldering: moderately hard soldering: moderately gas shielded welding: moderately burnishing: good Application: For live springs and contacts, electrodes for resistance welding.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.8 - 8.92 g/cm³

Show Material materials with Densidad of 8.8 - 8.92 g/cm³

Mecánica

PropertyTemperatureValue

Elongación

20.0 °C

8 %

Show Material materials with Elongación of 8 %

Elongation A100

20.0 °C

2 - 3 %

Show Material materials with Elongation A100 of 2 - 3 %

Elongation A11.3

20.0 °C

5 - 6 %

Show Material materials with Elongation A11.3 of 5 - 6 %

Límite elástico Rp 0,2

20.0 °C

420 MPa

Show Material materials with Límite elástico Rp 0,2 of 420 MPa

Módulo elástico

20.0 °C

130 GPa

Show Material materials with Módulo elástico of 130 GPa

Resistencia a la tracción

20.0 °C

470 MPa

Show Material materials with Resistencia a la tracción of 470 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Calor específico of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Coeficiente de dilatación térmica

100.0 °C

1.63E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K

200.0 °C

1.7E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K

300.0 °C

1.76E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K

Conductividad térmica

20.0 °C

320 W/(m·K)

Show Material materials with Conductividad térmica of 320 W/(m·K)

Temperatura de fusión

855 - 1090 °C

Show Material materials with Temperatura de fusión of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

4.30E+7 - 4.60E+7 S/m

Show Material materials with Conductividad eléctrica of 4.30E+7 - 4.60E+7 S/m

Specific Electrical conductivity

74 - 79 % IACS

Show Material materials with Specific Electrical conductivity of 74 - 79 % IACS

Chemical properties

PropertyValue

Circonio

0.03 - 0.3 %

Show Material materials with Circonio of 0.03 - 0.3 %

Cromo

0.5 - 1.2 %

Show Material materials with Cromo of 0.5 - 1.2 %

Hierro

0.08 %

Show Material materials with Hierro of 0.08 %

Silicona

0.1 %

Show Material materials with Silicona of 0.1 %