General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 - 8.92 g/cm³ Show Material materials with Densidad of 8.9 - 8.92 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 65 - 90 [-] Show Material materials with Dureza Brinell of 65 - 90 [-] |
Dureza Vickers | 20.0 °C | 70 - 95 [-] Show Material materials with Dureza Vickers of 70 - 95 [-] |
Elongación | 20.0 °C | 20 - 30 % Show Material materials with Elongación of 20 - 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 60 - 150 MPa Show Material materials with Límite elástico Rp 0,2 of 60 - 150 MPa |
Módulo elástico | 20.0 °C | 130 GPa Show Material materials with Módulo elástico of 130 GPa |
Resistencia a la tracción | 20.0 °C | 200 - 250 MPa Show Material materials with Resistencia a la tracción of 200 - 250 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 100.0 °C | 1.63E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K | |
200.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
300.0 °C | 1.76E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K | ||
Conductividad térmica | 20.0 °C | 320 W/(m·K) Show Material materials with Conductividad térmica of 320 W/(m·K) | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.30E+7 S/m Show Material materials with Conductividad eléctrica of 4.30E+7 S/m |
Specific Electrical conductivity | 74 % IACS Show Material materials with Specific Electrical conductivity of 74 % IACS |
Chemical properties
Property | Value |
---|---|
Circonio | 0.03 - 0.3 % Show Material materials with Circonio of 0.03 - 0.3 % |
Cromo | 0.5 - 1.2 % Show Material materials with Cromo of 0.5 - 1.2 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |