General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 - 8.91 g/cm³ Show Material materials with Densidad of 8.9 - 8.91 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 120 - 180 [-] Show Material materials with Dureza Brinell of 120 - 180 [-] | |
Dureza Vickers | 20.0 °C | 125 - 185 [-] Show Material materials with Dureza Vickers of 125 - 185 [-] | |
Elongación | 20.0 °C | 8 - 15 % Show Material materials with Elongación of 8 - 15 % | |
Elongation A10 | 20.0 °C | 7 - 13 % Show Material materials with Elongation A10 of 7 - 13 % | |
Elongation A100 | 20.0 °C | 11 % Show Material materials with Elongation A100 of 11 % | |
Límite elástico Rp 0,2 | 20.0 °C | 270 - 380 MPa Show Material materials with Límite elástico Rp 0,2 of 270 - 380 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 20.0 °C | 360 - 470 MPa Show Material materials with Resistencia a la tracción of 360 - 470 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 100.0 °C | 1.63E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K | |
200.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
300.0 °C | 1.76E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.76E-5 1/K | ||
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Circonio | 0.03 - 0.3 % Show Material materials with Circonio of 0.03 - 0.3 % |
Cromo | 0.5 - 1.2 % Show Material materials with Cromo of 0.5 - 1.2 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |