General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.86 - 8.9 g/cm³ Show Material materials with Densidad of 8.86 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Elongación | 20.0 °C | 15 % Show Material materials with Elongación of 15 % | |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % | |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % | |
Límite elástico Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 127 GPa Show Material materials with Módulo elástico of 127 GPa | |
Resistencia a la tracción | 20.0 °C | 290 MPa Show Material materials with Resistencia a la tracción of 290 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 - 380 J/(kg·K) Show Material materials with Calor específico of 377 - 380 J/(kg·K) | |
100.0 °C | 386 J/(kg·K) Show Material materials with Calor específico of 386 J/(kg·K) | ||
200.0 °C | 398 J/(kg·K) Show Material materials with Calor específico of 398 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
300.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
Conductividad térmica | -200.0 °C | 128 W/(m·K) Show Material materials with Conductividad térmica of 128 W/(m·K) | |
20.0 °C | 234 - 243 W/(m·K) Show Material materials with Conductividad térmica of 234 - 243 W/(m·K) | ||
200.0 °C | 272 W/(m·K) Show Material materials with Conductividad térmica of 272 W/(m·K) | ||
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 3.30E+7 S/m Show Material materials with Conductividad eléctrica of 3.30E+7 S/m |
Specific Electrical conductivity | 57 % IACS Show Material materials with Specific Electrical conductivity of 57 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 94 - 96 % Show Material materials with Cobre of 94 - 96 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |