General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.67 - 8.7 g/cm³ Show Material materials with Densidad of 8.67 - 8.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Elongación | 20.0 °C | 7 % Show Material materials with Elongación of 7 % |
Elongation A100 | 20.0 °C | 5 % Show Material materials with Elongation A100 of 5 % |
Elongation A11.3 | 20.0 °C | 6 % Show Material materials with Elongation A11.3 of 6 % |
Límite elástico Rp 0,2 | 20.0 °C | 300 - 410 MPa Show Material materials with Límite elástico Rp 0,2 of 300 - 410 MPa |
Módulo de cizallamiento | 20.0 °C | 44 GPa Show Material materials with Módulo de cizallamiento of 44 GPa |
Módulo elástico | 20.0 °C | 119 GPa Show Material materials with Módulo elástico of 119 GPa |
100.0 °C | 116 GPa Show Material materials with Módulo elástico of 116 GPa | |
200.0 °C | 111 GPa Show Material materials with Módulo elástico of 111 GPa | |
300.0 °C | 106 GPa Show Material materials with Módulo elástico of 106 GPa | |
400.0 °C | 100 GPa Show Material materials with Módulo elástico of 100 GPa | |
500.0 °C | 91 GPa Show Material materials with Módulo elástico of 91 GPa | |
600.0 °C | 81 GPa Show Material materials with Módulo elástico of 81 GPa | |
700.0 °C | 71 GPa Show Material materials with Módulo elástico of 71 GPa | |
Resistencia a la tracción | 20.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 - 380 J/(kg·K) Show Material materials with Calor específico of 377 - 380 J/(kg·K) | |
100.0 °C | 398 J/(kg·K) Show Material materials with Calor específico of 398 J/(kg·K) | ||
200.0 °C | 410 J/(kg·K) Show Material materials with Calor específico of 410 J/(kg·K) | ||
300.0 °C | 419 J/(kg·K) Show Material materials with Calor específico of 419 J/(kg·K) | ||
400.0 °C | 431 J/(kg·K) Show Material materials with Calor específico of 431 J/(kg·K) | ||
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 142 W/(m·K) Show Material materials with Conductividad térmica of 142 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.90E+7 S/m Show Material materials with Conductividad eléctrica of 1.90E+7 S/m |
Resistividad eléctrica | 20.0 °C | 5.3E-8 Ω·m Show Material materials with Resistividad eléctrica of 5.3E-8 Ω·m |
Specific Electrical conductivity | 33 % IACS Show Material materials with Specific Electrical conductivity of 33 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 79 - 81 % Show Material materials with Cobre of 79 - 81 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |