General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.24 - 8.3 g/cm³ Show Material materials with Densidad of 8.24 - 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Brinell of 120 - 150 [-] |
Dureza Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Dureza Vickers of 125 - 155 [-] |
Módulo elástico | 20.0 °C | 93 GPa Show Material materials with Módulo elástico of 93 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 63 W/(m·K) Show Material materials with Conductividad térmica of 63 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.80E+6 S/m Show Material materials with Conductividad eléctrica of 7.80E+6 S/m |
Specific Electrical conductivity | 13 % IACS Show Material materials with Specific Electrical conductivity of 13 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 1.3 % Show Material materials with Aluminio of 0.3 - 1.3 % |
Cobre | 59 - 61.5 % Show Material materials with Cobre of 59 - 61.5 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.6 - 1.8 % Show Material materials with Manganeso of 0.6 - 1.8 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Plomo | 1 % Show Material materials with Plomo of 1 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |