General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 95 - 130 [-] Show Material materials with Dureza Brinell of 95 - 130 [-] |
Elongación | 20.0 °C | 5 % Show Material materials with Elongación of 5 % |
Elongation A10 | 20.0 °C | 3 % Show Material materials with Elongation A10 of 3 % |
Elongation A100 | 20.0 °C | 2 % Show Material materials with Elongation A100 of 2 % |
Elongation A11.3 | 20.0 °C | 3 % Show Material materials with Elongation A11.3 of 3 % |
Límite elástico Rp 0,2 | 20.0 °C | 240 - 250 MPa Show Material materials with Límite elástico Rp 0,2 of 240 - 250 MPa |
Módulo elástico | 20.0 °C | 115 GPa Show Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 20.0 °C | 300 MPa Show Material materials with Resistencia a la tracción of 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Conductividad térmica | 20.0 °C | 350 W/(m·K) Show Material materials with Conductividad térmica of 350 W/(m·K) | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 5.00E+7 S/m Show Material materials with Conductividad eléctrica of 5.00E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value |
---|---|
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Plomo | 0.7 - 1.5 % Show Material materials with Plomo of 0.7 - 1.5 % |