General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 - 8.41 g/cm³ Show Material materials with Densidad of 8.4 - 8.41 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Dureza Brinell | 20.0 °C | 70 - 100 [-] Show Material materials with Dureza Brinell of 70 - 100 [-] |
Dureza Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Dureza Vickers of 75 - 105 [-] |
Elongación | 20.0 °C | 35 - 55 % Show Material materials with Elongación of 35 - 55 % |
150.0 °C | 62 % Show Material materials with Elongación of 62 % | |
200.0 °C | 45 % Show Material materials with Elongación of 45 % | |
250.0 °C | 28 % Show Material materials with Elongación of 28 % | |
Límite elástico Rp 0,2 | 20.0 °C | 125 - 250 MPa Show Material materials with Límite elástico Rp 0,2 of 125 - 250 MPa |
150.0 °C | 130 MPa Show Material materials with Límite elástico Rp 0,2 of 130 MPa | |
200.0 °C | 135 MPa Show Material materials with Límite elástico Rp 0,2 of 135 MPa | |
250.0 °C | 127 MPa Show Material materials with Límite elástico Rp 0,2 of 127 MPa | |
Límite elástico Rp 1,0 | 20.0 °C | 137 MPa Show Material materials with Límite elástico Rp 1,0 of 137 MPa |
150.0 °C | 144 MPa Show Material materials with Límite elástico Rp 1,0 of 144 MPa | |
200.0 °C | 146 MPa Show Material materials with Límite elástico Rp 1,0 of 146 MPa | |
250.0 °C | 135 MPa Show Material materials with Límite elástico Rp 1,0 of 135 MPa | |
Módulo de cizallamiento | 20.0 °C | 37 GPa Show Material materials with Módulo de cizallamiento of 37 GPa |
Módulo elástico | -195.0 °C | 108 GPa Show Material materials with Módulo elástico of 108 GPa |
-100.0 °C | 106 GPa Show Material materials with Módulo elástico of 106 GPa | |
20.0 °C | 102 - 105 GPa Show Material materials with Módulo elástico of 102 - 105 GPa | |
50.0 °C | 100 GPa Show Material materials with Módulo elástico of 100 GPa | |
100.0 °C | 93 - 99 GPa Show Material materials with Módulo elástico of 93 - 99 GPa | |
150.0 °C | 91 GPa Show Material materials with Módulo elástico of 91 GPa | |
200.0 °C | 89 - 94 GPa Show Material materials with Módulo elástico of 89 - 94 GPa | |
250.0 °C | 83 GPa Show Material materials with Módulo elástico of 83 GPa | |
300.0 °C | 89 GPa Show Material materials with Módulo elástico of 89 GPa | |
400.0 °C | 83 GPa Show Material materials with Módulo elástico of 83 GPa | |
500.0 °C | 74 GPa Show Material materials with Módulo elástico of 74 GPa | |
600.0 °C | 64 GPa Show Material materials with Módulo elástico of 64 GPa | |
700.0 °C | 54 GPa Show Material materials with Módulo elástico of 54 GPa | |
Resistencia a la tracción | 20.0 °C | 340 - 374 MPa Show Material materials with Resistencia a la tracción of 340 - 374 MPa |
150.0 °C | 314 MPa Show Material materials with Resistencia a la tracción of 314 MPa | |
200.0 °C | 271 MPa Show Material materials with Resistencia a la tracción of 271 MPa | |
250.0 °C | 221 MPa Show Material materials with Resistencia a la tracción of 221 MPa | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 375 - 377 J/(kg·K) Show Material materials with Calor específico of 375 - 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 109 - 117 W/(m·K) Show Material materials with Conductividad térmica of 109 - 117 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.39E+7 - 1.50E+7 S/m Show Material materials with Conductividad eléctrica of 1.39E+7 - 1.50E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.7E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.7E-8 Ω·m |
Specific Electrical conductivity | 24 - 26 % IACS Show Material materials with Specific Electrical conductivity of 24 - 26 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 59.5 - 61.5 % Show Material materials with Cobre of 59.5 - 61.5 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.2 - 0.3 % Show Material materials with Plomo of 0.2 - 0.3 % |