Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.6 - 8.62 g/cm³ Show Material materials with Densidad of 8.6 - 8.62 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Límite elástico Rp 0,2 | 20.0 °C | 580 - 600 MPa Show Material materials with Límite elástico Rp 0,2 of 580 - 600 MPa | |
Módulo elástico | 20.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | |
Resistencia a la tracción | 20.0 °C | 650 MPa Show Material materials with Resistencia a la tracción of 650 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 300.0 °C | 1.95E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.95E-5 1/K | |
Conductividad térmica | 20.0 °C | 42 W/(m·K) Show Material materials with Conductividad térmica of 42 W/(m·K) | |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.20E+6 S/m Show Material materials with Conductividad eléctrica of 4.20E+6 S/m |
Specific Electrical conductivity | 7 % IACS Show Material materials with Specific Electrical conductivity of 7 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 56 - 58 % Show Material materials with Cobre of 56 - 58 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 11 - 13 % Show Material materials with Níquel of 11 - 13 % |
Plomo | 0.5 - 1.5 % Show Material materials with Plomo of 0.5 - 1.5 % |