General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.89 - 8.9 g/cm³ Show Material materials with Densidad of 8.89 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Límite elástico Rp 0,2 | 20.0 °C | 580 MPa Show Material materials with Límite elástico Rp 0,2 of 580 MPa | |
Módulo elástico | 20.0 °C | 103 GPa Show Material materials with Módulo elástico of 103 GPa | |
Resistencia a la tracción | 20.0 °C | 640 MPa Show Material materials with Resistencia a la tracción of 640 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) |
200.0 °C | 410 J/(kg·K) Show Material materials with Calor específico of 410 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.63E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K |
300.0 °C | 1.73E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.73E-5 1/K | |
Conductividad térmica | 20.0 °C | 86.5 - 87 W/(m·K) Show Material materials with Conductividad térmica of 86.5 - 87 W/(m·K) |
200.0 °C | 109 W/(m·K) Show Material materials with Conductividad térmica of 109 W/(m·K) | |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.20E+7 S/m Show Material materials with Conductividad eléctrica of 1.20E+7 S/m |
Specific Electrical conductivity | 21 % IACS Show Material materials with Specific Electrical conductivity of 21 % IACS |
Chemical properties
Property | Value |
---|---|
Estaño | 3.5 - 4.5 % Show Material materials with Estaño of 3.5 - 4.5 % |
Fósforo | 0.01 - 0.4 % Show Material materials with Fósforo of 0.01 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 3.5 - 4.5 % Show Material materials with Plomo of 3.5 - 4.5 % |
Telurio | 0.2 % Show Material materials with Telurio of 0.2 % |
Zinc | 3.5 - 4.5 % Show Material materials with Zinc of 3.5 - 4.5 % |