General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 180 [-] Show Material materials with Dureza Brinell of 180 [-] | |
Dureza Vickers | 20.0 °C | 190 [-] Show Material materials with Dureza Vickers of 190 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa | |
Resistencia a la tracción | 20.0 °C | 700 MPa Show Material materials with Resistencia a la tracción of 700 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 27 W/(m·K) Show Material materials with Conductividad térmica of 27 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.00E+6 S/m Show Material materials with Conductividad eléctrica of 4.00E+6 S/m |
Specific Electrical conductivity | 6.9 % IACS Show Material materials with Specific Electrical conductivity of 6.9 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 5 - 7 % Show Material materials with Aluminio of 5 - 7 % |
Cobre | 63 - 65.5 % Show Material materials with Cobre of 63 - 65.5 % |
Hierro | 2 - 3.5 % Show Material materials with Hierro of 2 - 3.5 % |
Manganeso | 3.5 - 5 % Show Material materials with Manganeso of 3.5 - 5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Plomo | 1 % Show Material materials with Plomo of 1 % |