Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 360 - 460 [-] Show Material materials with Dureza Vickers of 360 - 460 [-] |
Elongación | 20.0 °C | 1 - 2 % Show Material materials with Elongación of 1 - 2 % |
Límite elástico Rp 0,2 | 20.0 °C | 1150 - 1300 MPa Show Material materials with Límite elástico Rp 0,2 of 1150 - 1300 MPa |
Resistencia a la tracción | 20.0 °C | 1190 - 1520 MPa Show Material materials with Resistencia a la tracción of 1190 - 1520 MPa |
Chemical properties
Property | Value |
---|---|
Berilio | 1.8 - 2 % Show Material materials with Berilio of 1.8 - 2 % |
Cobalto | 0.3 % Show Material materials with Cobalto of 0.3 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.2 - 0.6 % Show Material materials with Plomo of 0.2 - 0.6 % |