General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Densidad of 8.8 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Dureza Vickers | 20.0 °C | 110 - 140 [-] Show Material materials with Dureza Vickers of 110 - 140 [-] | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 20.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 300.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | |
Conductividad térmica | 20.0 °C | 368 W/(m·K) Show Material materials with Conductividad térmica of 368 W/(m·K) | |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 5.45E+7 S/m Show Material materials with Conductividad eléctrica of 5.45E+7 S/m |
Chemical properties
Property | Value |
---|---|
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Telurio | 0.4 - 0.7 % Show Material materials with Telurio of 0.4 - 0.7 % |