General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Densidad of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Dureza Vickers | 20.0 °C | 150 - 190 [-] Show Material materials with Dureza Vickers of 150 - 190 [-] | |
Elongación | 20.0 °C | 15 % Show Material materials with Elongación of 15 % | |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % | |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % | |
Límite elástico Rp 0,2 | 20.0 °C | 300 MPa Show Material materials with Límite elástico Rp 0,2 of 300 MPa | |
Módulo elástico | 23.0 °C | 120 - 140 GPa Show Material materials with Módulo elástico of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Resistencia a la tracción | 20.0 °C | 540 MPa Show Material materials with Resistencia a la tracción of 540 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Conductividad térmica | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Conductividad térmica of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Cobre | 45 - 48 % Show Material materials with Cobre of 45 - 48 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Plomo | 1 - 2.5 % Show Material materials with Plomo of 1 - 2.5 % |