EN 12166 Grade CuNi12Zn30Pb1 H130

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

Material CuNi12Zn30Pb1, mat. No. CW406J is an alloy of high strength and hardness. To the comparabel mark CuNi12Zn30Pb1, mat. No. 2.0780, acc. to DIN 17663 : 1983-12 applies: Strength is further increasable due to the high strain hardening capability. The material does not embrittle at low temperatures. Low electrical and thermal conductivity. The alloy is non-magnetic, corrosion resistance is better than for pure copper. Machinability improves by Pb-addition, ductility decreases and cold workabiliy deteriorates. Processing properties: warm forming: unfavorable cold forming: moderately machinability: good hard and soft soldering: very good TIG-welding: moderately burnishing: good Application: Particularly in precision engineering and in toolbuilding for turning and drilling parts, in electrical engineering and electronics as well as in shipbuilding and in construction trade.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.6 - 8.62 g/cm³

Show Material materials with Densidad of 8.6 - 8.62 g/cm³

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.32 [-]

Show Material materials with Coeficiente de Poisson of 0.32 [-]

Typical for Wrought Copper Nickel Silver Grade

Dureza Brinell

20.0 °C

130 - 155 [-]

Show Material materials with Dureza Brinell of 130 - 155 [-]

Dureza Vickers

20.0 °C

135 [-]

Show Material materials with Dureza Vickers of 135 [-]

Módulo elástico

20.0 °C

120 GPa

Show Material materials with Módulo elástico of 120 GPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

377 J/(kg·K)

Show Material materials with Calor específico of 377 J/(kg·K)

Typical for Wrought Copper Nickel Silver Grade

Coeficiente de dilatación térmica

300.0 °C

1.95E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.95E-5 1/K

Conductividad térmica

20.0 °C

42 W/(m·K)

Show Material materials with Conductividad térmica of 42 W/(m·K)

Temperatura de fusión

875 - 1135 °C

Show Material materials with Temperatura de fusión of 875 - 1135 °C

Typical for Wrought Copper Nickel Silver Grade

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

4.20E+6 S/m

Show Material materials with Conductividad eléctrica of 4.20E+6 S/m

Specific Electrical conductivity

7 % IACS

Show Material materials with Specific Electrical conductivity of 7 % IACS

Chemical properties

PropertyValue

Cobre

56 - 58 %

Show Material materials with Cobre of 56 - 58 %

Estaño

0.2 %

Show Material materials with Estaño of 0.2 %

Hierro

0.3 %

Show Material materials with Hierro of 0.3 %

Manganeso

0.5 %

Show Material materials with Manganeso of 0.5 %

Níquel

11 - 13 %

Show Material materials with Níquel of 11 - 13 %

Plomo

0.5 - 1.5 %

Show Material materials with Plomo of 0.5 - 1.5 %