General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 - 8.44 g/cm³ Show Material materials with Densidad of 8.4 - 8.44 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 55 - 85 [-] Show Material materials with Dureza Brinell of 55 - 85 [-] | |
Dureza Vickers | 20.0 °C | 60 - 105 [-] Show Material materials with Dureza Vickers of 60 - 105 [-] | |
Elongación | 20.0 °C | 44 - 45 % Show Material materials with Elongación of 44 - 45 % | |
100.0 °C | 45 % Show Material materials with Elongación of 45 % | ||
150.0 °C | 50 % Show Material materials with Elongación of 50 % | ||
200.0 °C | 47 % Show Material materials with Elongación of 47 % | ||
Elongation A10 | 20.0 °C | 40 % Show Material materials with Elongation A10 of 40 % | |
Elongation A100 | 20.0 °C | 30 - 35 % Show Material materials with Elongation A100 of 30 - 35 % | |
Límite elástico Rp 0,2 | 20.0 °C | 130 - 226 MPa Show Material materials with Límite elástico Rp 0,2 of 130 - 226 MPa | |
100.0 °C | 221 MPa Show Material materials with Límite elástico Rp 0,2 of 221 MPa | ||
150.0 °C | 226 MPa Show Material materials with Límite elástico Rp 0,2 of 226 MPa | ||
200.0 °C | 206 MPa Show Material materials with Límite elástico Rp 0,2 of 206 MPa | ||
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 110 GPa Show Material materials with Módulo elástico of 110 GPa | |
100.0 °C | 106 GPa Show Material materials with Módulo elástico of 106 GPa | ||
200.0 °C | 102 GPa Show Material materials with Módulo elástico of 102 GPa | ||
300.0 °C | 97 GPa Show Material materials with Módulo elástico of 97 GPa | ||
400.0 °C | 89 GPa Show Material materials with Módulo elástico of 89 GPa | ||
500.0 °C | 79 GPa Show Material materials with Módulo elástico of 79 GPa | ||
Resistencia a la tracción | 20.0 °C | 280 - 450 MPa Show Material materials with Resistencia a la tracción of 280 - 450 MPa | |
100.0 °C | 341 MPa Show Material materials with Resistencia a la tracción of 341 MPa | ||
150.0 °C | 327 MPa Show Material materials with Resistencia a la tracción of 327 MPa | ||
200.0 °C | 315 MPa Show Material materials with Resistencia a la tracción of 315 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 150.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | |
300.0 °C | 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1E-5 1/K | ||
650.0 °C | 2.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K | ||
800.0 °C | 2.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | ||
Conductividad térmica | -200.0 °C | 50 W/(m·K) Show Material materials with Conductividad térmica of 50 W/(m·K) | |
20.0 °C | 120 W/(m·K) Show Material materials with Conductividad térmica of 120 W/(m·K) | ||
200.0 °C | 142 W/(m·K) Show Material materials with Conductividad térmica of 142 W/(m·K) | ||
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.50E+7 S/m Show Material materials with Conductividad eléctrica of 1.50E+7 S/m |
200.0 °C | 1.20E+7 S/m Show Material materials with Conductividad eléctrica of 1.20E+7 S/m | |
Resistividad eléctrica | 20.0 °C | 6.6E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.6E-8 Ω·m |
200.0 °C | 8.3E-8 Ω·m Show Material materials with Resistividad eléctrica of 8.3E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 62 - 64 % Show Material materials with Cobre of 62 - 64 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |