General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.45 - 8.5 g/cm³ Show Material materials with Densidad of 8.45 - 8.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 100 - 140 [-] Show Material materials with Dureza Brinell of 100 - 140 [-] | |
Dureza Vickers | 20.0 °C | 100 - 150 [-] Show Material materials with Dureza Vickers of 100 - 150 [-] | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 110 GPa Show Material materials with Módulo elástico of 110 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 113 W/(m·K) Show Material materials with Conductividad térmica of 113 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.47E+7 S/m Show Material materials with Conductividad eléctrica of 1.47E+7 S/m |
Specific Electrical conductivity | 25 % IACS Show Material materials with Specific Electrical conductivity of 25 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 62.5 - 64 % Show Material materials with Cobre of 62.5 - 64 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.8 - 1.6 % Show Material materials with Plomo of 0.8 - 1.6 % |