General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.46 - 8.5 g/cm³ Show Material materials with Densidad of 8.46 - 8.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 70 - 120 [-] Show Material materials with Dureza Brinell of 70 - 120 [-] |
Dureza Vickers | 20.0 °C | 80 - 130 [-] Show Material materials with Dureza Vickers of 80 - 130 [-] |
Módulo de cizallamiento | 20.0 °C | 39 GPa Show Material materials with Módulo de cizallamiento of 39 GPa |
Módulo elástico | 20.0 °C | 105 - 110 GPa Show Material materials with Módulo elástico of 105 - 110 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 200.0 °C | 2.04E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.04E-5 1/K | |
Conductividad térmica | 20.0 °C | 113 - 116 W/(m·K) Show Material materials with Conductividad térmica of 113 - 116 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.47E+7 S/m Show Material materials with Conductividad eléctrica of 1.47E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.8E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.8E-8 Ω·m |
Specific Electrical conductivity | 25 % IACS Show Material materials with Specific Electrical conductivity of 25 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 62 - 63.5 % Show Material materials with Cobre of 62 - 63.5 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 1.6 - 2.5 % Show Material materials with Plomo of 1.6 - 2.5 % |