General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 110 - 160 [-] Show Material materials with Dureza Brinell of 110 - 160 [-] | |
Dureza Vickers | 20.0 °C | 120 - 170 [-] Show Material materials with Dureza Vickers of 120 - 170 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 340 MPa Show Material materials with Límite elástico Rp 0,2 of 340 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 23.0 °C | 100 - 125 GPa Show Material materials with Módulo elástico of 100 - 125 GPa | Typical for Wrought Copper Brass |
Resistencia a la tracción | 20.0 °C | 440 MPa Show Material materials with Resistencia a la tracción of 440 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Conductividad térmica of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 62 - 63.5 % Show Material materials with Cobre of 62 - 63.5 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 1.6 - 2.5 % Show Material materials with Plomo of 1.6 - 2.5 % |