General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.47 - 8.5 g/cm³ Show Material materials with Densidad of 8.47 - 8.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 70 - 120 [-] Show Material materials with Dureza Brinell of 70 - 120 [-] | |
Dureza Vickers | 20.0 °C | 80 - 130 [-] Show Material materials with Dureza Vickers of 80 - 130 [-] | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 102 GPa Show Material materials with Módulo elástico of 102 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 200.0 °C | 2.06E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.06E-5 1/K | |
Conductividad térmica | 20.0 °C | 100 W/(m·K) Show Material materials with Conductividad térmica of 100 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.30E+7 S/m Show Material materials with Conductividad eléctrica of 1.30E+7 S/m |
Resistividad eléctrica | 20.0 °C | 7.7E-8 Ω·m Show Material materials with Resistividad eléctrica of 7.7E-8 Ω·m |
Specific Electrical conductivity | 22 % IACS Show Material materials with Specific Electrical conductivity of 22 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 60 - 62 % Show Material materials with Cobre of 60 - 62 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 2.5 - 3.5 % Show Material materials with Plomo of 2.5 - 3.5 % |