Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 20.0 °C | 145 - 185 [-] Show Material materials with Dureza Vickers of 145 - 185 [-] | |
Elongación | 20.0 °C | 8 % Show Material materials with Elongación of 8 % | |
Elongation A10 | 20.0 °C | 6 % Show Material materials with Elongation A10 of 6 % | |
Elongation A100 | 20.0 °C | 4 % Show Material materials with Elongation A100 of 4 % | |
Límite elástico Rp 0,2 | 20.0 °C | 390 - 400 MPa Show Material materials with Límite elástico Rp 0,2 of 390 - 400 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 23.0 °C | 100 - 125 GPa Show Material materials with Módulo elástico of 100 - 125 GPa | Typical for Wrought Copper Brass |
Resistencia a la tracción | 20.0 °C | 490 - 520 MPa Show Material materials with Resistencia a la tracción of 490 - 520 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Conductividad térmica of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 57 - 59 % Show Material materials with Cobre of 57 - 59 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 3.5 - 4.2 % Show Material materials with Plomo of 3.5 - 4.2 % |