General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 - 8.44 g/cm³ Show Material materials with Densidad of 8.4 - 8.44 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 20.0 °C | 110 - 165 [-] Show Material materials with Dureza Vickers of 110 - 165 [-] | |
Elongación | -183.0 °C | 33 % Show Material materials with Elongación of 33 % | |
-78.0 °C | 27 % Show Material materials with Elongación of 27 % | ||
20.0 °C | 10 - 28 % Show Material materials with Elongación of 10 - 28 % | ||
Elongation A10 | 20.0 °C | 8 % Show Material materials with Elongation A10 of 8 % | |
Elongation A100 | 20.0 °C | 6 % Show Material materials with Elongation A100 of 6 % | |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 96 - 97 GPa Show Material materials with Módulo elástico of 96 - 97 GPa | |
Resistencia a la tracción | -183.0 °C | 595 MPa Show Material materials with Resistencia a la tracción of 595 MPa | |
-78.0 °C | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa | ||
20.0 °C | 400 - 450 MPa Show Material materials with Resistencia a la tracción of 400 - 450 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2E-5 1/K | |
300.0 °C | 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1E-5 1/K | ||
Conductividad térmica | -200.0 °C | 50 W/(m·K) Show Material materials with Conductividad térmica of 50 W/(m·K) | |
20.0 °C | 113 - 123 W/(m·K) Show Material materials with Conductividad térmica of 113 - 123 W/(m·K) | ||
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.49E+7 - 1.50E+7 S/m Show Material materials with Conductividad eléctrica of 1.49E+7 - 1.50E+7 S/m |
200.0 °C | 1.20E+7 S/m Show Material materials with Conductividad eléctrica of 1.20E+7 S/m | |
Resistividad eléctrica | 20.0 °C | 6.6E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.6E-8 Ω·m |
200.0 °C | 8.3E-8 Ω·m Show Material materials with Resistividad eléctrica of 8.3E-8 Ω·m | |
Specific Electrical conductivity | 25 - 25.7 % IACS Show Material materials with Specific Electrical conductivity of 25 - 25.7 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 57 - 59 % Show Material materials with Cobre of 57 - 59 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 1.6 - 2.5 % Show Material materials with Plomo of 1.6 - 2.5 % |