General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.1 - 8.3 g/cm³ Show Material materials with Densidad of 8.1 - 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 90 - 150 [-] Show Material materials with Dureza Brinell of 90 - 150 [-] |
Dureza Vickers | 20.0 °C | 100 - 135 [-] Show Material materials with Dureza Vickers of 100 - 135 [-] |
Módulo de cizallamiento | 20.0 °C | 36 GPa Show Material materials with Módulo de cizallamiento of 36 GPa |
Módulo elástico | 20.0 °C | 95 GPa Show Material materials with Módulo elástico of 95 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 200.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | |
Conductividad térmica | 20.0 °C | 67 W/(m·K) Show Material materials with Conductividad térmica of 67 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 8.70E+6 S/m Show Material materials with Conductividad eléctrica of 8.70E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.15E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.15E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Cobre | 57 - 59 % Show Material materials with Cobre of 57 - 59 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Plomo | 1 - 2 % Show Material materials with Plomo of 1 - 2 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |