EN 12166 Grade CuBe2 TB00

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

CuBe2, mat. No CW101C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBe2, mat. No 2.1247, acc. to DIN 17666 : 1983-12 applies: It is an alloy of optimal hardenability for highest requirements to strength, elasticity, abrasion and fatigue resistance. CuBe2 shows mean electrical and favorable thermal conductivity. The material does not show any embrittlement at lower temperatures (up to -200°C) as well as no stress corrosion sensitivity. The temperature for removal of workhardening approximates 350°C. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: For bearing jewels and screws, tensioning belts and wires, membranes, balance springs and drawn parts for watches, all types of springs. Individual parts for HF- and NF- special couplers, wear-resistant worms and gear-wheels, high-stress solid components, non-magnetic and spark-safe. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.3 g/cm³

Show Material materials with Densidad of 8.3 g/cm³

Mecánica

PropertyTemperatureValueComment

Dureza Brinell

20.0 °C

85 - 120 [-]

Show Material materials with Dureza Brinell of 85 - 120 [-]

Dureza Vickers

20.0 °C

90 - 160 [-]

Show Material materials with Dureza Vickers of 90 - 160 [-]

Elongación

20.0 °C

20 - 35 %

Show Material materials with Elongación of 20 - 35 %

Elongation A10

20.0 °C

25 - 30 %

Show Material materials with Elongation A10 of 25 - 30 %

Elongation A100

20.0 °C

25 - 35 %

Show Material materials with Elongation A100 of 25 - 35 %

Límite elástico Rp 0,2

20.0 °C

140 - 220 MPa

Show Material materials with Límite elástico Rp 0,2 of 140 - 220 MPa

Módulo elástico

23.0 °C

110 - 130 GPa

Show Material materials with Módulo elástico of 110 - 130 GPa

Typical for Wrought Copper High Copper Alloy

Resistencia a la tracción

20.0 °C

390 - 540 MPa

Show Material materials with Resistencia a la tracción of 390 - 540 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Calor específico of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Coeficiente de dilatación térmica

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper High Copper Alloy

Temperatura de fusión

855 - 1090 °C

Show Material materials with Temperatura de fusión of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Chemical properties

PropertyValue

Berilio

1.8 - 2.1 %

Show Material materials with Berilio of 1.8 - 2.1 %

Cobalto

0.3 %

Show Material materials with Cobalto of 0.3 %

Hierro

0.2 %

Show Material materials with Hierro of 0.2 %

Níquel

0.3 %

Show Material materials with Níquel of 0.3 %