General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 [-] Show Material materials with Dureza Brinell of 120 [-] |
Dureza Vickers | 20.0 °C | 125 - 130 [-] Show Material materials with Dureza Vickers of 125 - 130 [-] |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 59 - 60 % Show Material materials with Cobre of 59 - 60 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.8 - 1.6 % Show Material materials with Plomo of 0.8 - 1.6 % |