Mecánica
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 59 - 60 % Show Material materials with Cobre of 59 - 60 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.8 - 1.6 % Show Material materials with Plomo of 0.8 - 1.6 % |