EN 12167 Grade CuZn39Pb3 O60

View suppliers (30)
Want to keep this datasheet? Save it now in your required format

Description

Material CuZn39Pb3, mat. No. CW614N, is an unhardenable wrought alloy. to the comparable make CuZn39Pb3, mat. No. 2.0401 acc. to DIN 17660 : 1983-12 applies: High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for unleaded brass of the same Zn-content. Machinability is improved by Pb-addition. Corrosion resistance to water, several saline solutions and organic liquids is also lower than for unleaded alloys of the same zinc-content. Processing properties: warm forming: very good cold forming: unfavorable machinability: very good hard soldering: moderately soft soldering: very good TIG-welding: unfavorable burnishing: very good Application: Main alloy of the brass materials for machining on automats. Use for all types of form turning parts, in precision engineering as well as in watch and electrical industry.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.4 - 8.47 g/cm³

Show Material materials with Densidad of 8.4 - 8.47 g/cm³

Mecánica

PropertyTemperatureValueComment

Dureza Brinell

20.0 °C

80 - 115 [-]

Show Material materials with Dureza Brinell of 80 - 115 [-]

Dureza Vickers

20.0 °C

85 - 120 [-]

Show Material materials with Dureza Vickers of 85 - 120 [-]

Elongación

-196.0 °C

40 %

Show Material materials with Elongación of 40 %

-78.0 °C

34 %

Show Material materials with Elongación of 34 %

20.0 °C

25 - 33 %

Show Material materials with Elongación of 25 - 33 %

Límite elástico Rp 0,2

20.0 °C

250 MPa

Show Material materials with Límite elástico Rp 0,2 of 250 MPa

Módulo de cizallamiento

23.0 °C

40 GPa

Show Material materials with Módulo de cizallamiento of 40 GPa

Typical for Wrought Copper Brass

Módulo elástico

20.0 °C

96 - 97 GPa

Show Material materials with Módulo elástico of 96 - 97 GPa

Resistencia a la tracción

-196.0 °C

575 MPa

Show Material materials with Resistencia a la tracción of 575 MPa

-78.0 °C

460 MPa

Show Material materials with Resistencia a la tracción of 460 MPa

20.0 °C

360 - 425 MPa

Show Material materials with Resistencia a la tracción of 360 - 425 MPa

Unlock all property charts

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

377 J/(kg·K)

Show Material materials with Calor específico of 377 J/(kg·K)

Coeficiente de dilatación térmica

100.0 °C

1.93E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.93E-5 1/K

200.0 °C

2.1E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.1E-5 1/K

300.0 °C

2.14E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.14E-5 1/K

800.0 °C

2.47E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.47E-5 1/K

Unlock all property charts

Conductividad térmica

-200.0 °C

50 W/(m·K)

Show Material materials with Conductividad térmica of 50 W/(m·K)

20.0 °C

113 - 123 W/(m·K)

Show Material materials with Conductividad térmica of 113 - 123 W/(m·K)

Unlock all property charts

Temperatura de fusión

875 - 1075 °C

Show Material materials with Temperatura de fusión of 875 - 1075 °C

Typical for Wrought Copper Brass

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

1.46E+7 - 1.50E+7 S/m

Show Material materials with Conductividad eléctrica of 1.46E+7 - 1.50E+7 S/m

200.0 °C

1.20E+7 S/m

Show Material materials with Conductividad eléctrica of 1.20E+7 S/m

Unlock all property charts

Resistividad eléctrica

20.0 °C

6.6E-8 Ω·m

Show Material materials with Resistividad eléctrica of 6.6E-8 Ω·m

200.0 °C

8.3E-8 Ω·m

Show Material materials with Resistividad eléctrica of 8.3E-8 Ω·m

Unlock all property charts

Specific Electrical conductivity

25 - 25.2 % IACS

Show Material materials with Specific Electrical conductivity of 25 - 25.2 % IACS

Chemical properties

PropertyValue

Aluminio

0.05 %

Show Material materials with Aluminio of 0.05 %

Cobre

57 - 59 %

Show Material materials with Cobre of 57 - 59 %

Estaño

0.3 %

Show Material materials with Estaño of 0.3 %

Hierro

0.3 %

Show Material materials with Hierro of 0.3 %

Níquel

0.3 %

Show Material materials with Níquel of 0.3 %

Plomo

2.5 - 3.5 %

Show Material materials with Plomo of 2.5 - 3.5 %