General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.7 - 8.74 g/cm³ Show Material materials with Densidad of 8.7 - 8.74 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Dureza Brinell | 20.0 °C | 130 - 155 [-] Show Material materials with Dureza Brinell of 130 - 155 [-] | |
Dureza Vickers | 20.0 °C | 135 [-] Show Material materials with Dureza Vickers of 135 [-] | |
Módulo elástico | 20.0 °C | 130 GPa Show Material materials with Módulo elástico of 130 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 300.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | |
Conductividad térmica | 20.0 °C | 33 W/(m·K) Show Material materials with Conductividad térmica of 33 W/(m·K) | |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 3.20E+6 S/m Show Material materials with Conductividad eléctrica of 3.20E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 59.5 - 62.5 % Show Material materials with Cobre of 59.5 - 62.5 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % |
Níquel | 17 - 19 % Show Material materials with Níquel of 17 - 19 % |
Plomo | 0.5 - 1.5 % Show Material materials with Plomo of 0.5 - 1.5 % |