CuSn8, mat. No. CW453K, is comparable to the DIN-make CuSn8, mat. No. 2.1030, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Application: For friction elements, especially for thin-walled friction-bearing bushings and sliding strips as well as for beater bars. Increased abrasion and corrosion resistance compared to CuSn6. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.79 - 8.8 g/cm³

Show Material materials with Densidad of 8.79 - 8.8 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Elongación

20.0 °C

23 - 26 %

Show Material materials with Elongación of 23 - 26 %

Elongación A50

20.0 °C

20 - 23 %

Show Material materials with Elongación A50 of 20 - 23 %

Elongation A10

20.0 °C

22 %

Show Material materials with Elongation A10 of 22 %

Elongation A100

20.0 °C

18 %

Show Material materials with Elongation A100 of 18 %

Elongation A11.3

20.0 °C

22 %

Show Material materials with Elongation A11.3 of 22 %

Límite elástico Rp 0,2

20.0 °C

250 - 280 MPa

Show Material materials with Límite elástico Rp 0,2 of 250 - 280 MPa

Módulo elástico

20.0 °C

115 GPa

Show Material materials with Módulo elástico of 115 GPa

Resistencia a la tracción

20.0 °C

450 - 550 MPa

Show Material materials with Resistencia a la tracción of 450 - 550 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

20.0 °C

377 J/(kg·K)

Show Material materials with Calor específico of 377 J/(kg·K)

Coeficiente de dilatación térmica

100.0 °C

1.8E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K

300.0 °C

1.82E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.82E-5 1/K

400.0 °C

1.87E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.87E-5 1/K

650.0 °C

2.22E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.22E-5 1/K

800.0 °C

2.18E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.18E-5 1/K

Conductividad térmica

20.0 °C

67 W/(m·K)

Show Material materials with Conductividad térmica of 67 W/(m·K)

200.0 °C

81 W/(m·K)

Show Material materials with Conductividad térmica of 81 W/(m·K)

Unlock all property charts

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

7.00E+6 - 7.50E+6 S/m

Show Material materials with Conductividad eléctrica of 7.00E+6 - 7.50E+6 S/m

200.0 °C

6.50E+6 S/m

Show Material materials with Conductividad eléctrica of 6.50E+6 S/m

Unlock all property charts

Resistividad eléctrica

20.0 °C

1.33E-7 Ω·m

Show Material materials with Resistividad eléctrica of 1.33E-7 Ω·m

200.0 °C

1.54E-7 Ω·m

Show Material materials with Resistividad eléctrica of 1.54E-7 Ω·m

Unlock all property charts

Specific Electrical conductivity

12 - 13 % IACS

Show Material materials with Specific Electrical conductivity of 12 - 13 % IACS

Chemical properties

PropertyValue

Estaño

7.5 - 8.5 %

Show Material materials with Estaño of 7.5 - 8.5 %

Fósforo

0.01 - 0.4 %

Show Material materials with Fósforo of 0.01 - 0.4 %

Hierro

0.1 %

Show Material materials with Hierro of 0.1 %

Níquel

0.2 %

Show Material materials with Níquel of 0.2 %

Plomo

0.02 %

Show Material materials with Plomo of 0.02 %

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %