General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 90 - 125 [-] Show Material materials with Dureza Vickers of 90 - 125 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa |
Módulo elástico | 20.0 °C | 156 GPa Show Material materials with Módulo elástico of 156 GPa |
Resistencia a la tracción | 20.0 °C | 420 MPa Show Material materials with Resistencia a la tracción of 420 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 - 2.5 % Show Material materials with Hierro of 1.5 - 2.5 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Níquel | 29 - 32 % Show Material materials with Níquel of 29 - 32 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |