Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 55 % Show Material materials with Elongación of 55 % | |
Límite elástico Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Límite elástico Rp 0,2 of 120 MPa | |
Límite elástico Rp 1,0 | 20.0 °C | 130 MPa Show Material materials with Límite elástico Rp 1,0 of 130 MPa | |
50.0 °C | 130 MPa Show Material materials with Límite elástico Rp 1,0 of 130 MPa | ||
100.0 °C | 125 MPa Show Material materials with Límite elástico Rp 1,0 of 125 MPa | ||
150.0 °C | 125 MPa Show Material materials with Límite elástico Rp 1,0 of 125 MPa | ||
200.0 °C | 120 MPa Show Material materials with Límite elástico Rp 1,0 of 120 MPa | ||
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 110 GPa Show Material materials with Módulo elástico of 110 GPa | |
50.0 °C | 110 GPa Show Material materials with Módulo elástico of 110 GPa | ||
100.0 °C | 108 GPa Show Material materials with Módulo elástico of 108 GPa | ||
150.0 °C | 107 GPa Show Material materials with Módulo elástico of 107 GPa | ||
200.0 °C | 106 GPa Show Material materials with Módulo elástico of 106 GPa | ||
250.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa | ||
Resistencia a la tracción | 20.0 °C | 340 MPa Show Material materials with Resistencia a la tracción of 340 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Conductividad térmica of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.8 - 2.3 % Show Material materials with Aluminio of 1.8 - 2.3 % |
Arsénico | 0.02 - 0.06 % Show Material materials with Arsénico of 0.02 - 0.06 % |
Cobre | 76 - 79 % Show Material materials with Cobre of 76 - 79 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.07 % Show Material materials with Hierro of 0.07 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |