General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 85 - 95 [-] Show Material materials with Dureza Rockwell B of 85 - 95 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 72 - 80 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 72 - 80 [-] | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 585 - 690 MPa Show Material materials with Resistencia a la tracción of 585 - 690 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Estaño | 1.8 - 2.8 % Show Material materials with Estaño of 1.8 - 2.8 % |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 8.5 - 10.5 % Show Material materials with Níquel of 8.5 - 10.5 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |