Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Densidad of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Dureza Rockwell B | 23.0 °C | 29 - 45 [-] Show Material materials with Dureza Rockwell B of 29 - 45 [-] | |
Hardness, Rockwell F | 23.0 °C | 72 - 83 [-] Show Material materials with Hardness, Rockwell F of 72 - 83 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 35 - 46 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 35 - 46 [-] | |
Módulo elástico | 23.0 °C | 120 - 140 GPa Show Material materials with Módulo elástico of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Conductividad térmica | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Conductividad térmica of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Cobre | 53.5 - 56.5 % Show Material materials with Cobre of 53.5 - 56.5 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 16.5 - 19.5 % Show Material materials with Níquel of 16.5 - 19.5 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |