Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 38 - 65 [-] Show Material materials with Dureza Rockwell B of 38 - 65 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 42 - 60 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 42 - 60 [-] | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 23.0 °C | 100 - 125 GPa Show Material materials with Módulo elástico of 100 - 125 GPa | Typical for Wrought Copper Brass |
Resistencia a la tracción | 23.0 °C | 330 - 515 MPa Show Material materials with Resistencia a la tracción of 330 - 515 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Conductividad térmica of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Cobre | 78.5 - 81.5 % Show Material materials with Cobre of 78.5 - 81.5 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |