General
Property | Value | Condition |
---|---|---|
Densidad | 5.0 g/cm³ Show Material materials with Densidad of 5.0 g/cm³ | Moderate Strength |
Mecánica
Property | Value | Condition |
---|---|---|
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | Moderate Strength |
Límite elástico | 980.0 MPa Show Material materials with Límite elástico of 980.0 MPa | Moderate Strength |
Módulo elástico | 130.0 GPa Show Material materials with Módulo elástico of 130.0 GPa | Moderate Strength |
Resistencia a la tracción | 1070.0 MPa Show Material materials with Resistencia a la tracción of 1070.0 MPa | Moderate Strength |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 510.0 J/(kg·K) Show Material materials with Calor específico of 510.0 J/(kg·K) | Moderate Strength | |
Coeficiente de dilatación térmica | 9.6e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 9.6e-06 1/K | Moderate Strength | |
Conductividad térmica | 6.0 - 11.0 W/(m·K) Show Material materials with Conductividad térmica of 6.0 - 11.0 W/(m·K) | Typical for Titanium Beta Alloy | |
Temperatura de fusión | 1550.0 - 1815.0 °C Show Material materials with Temperatura de fusión of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 3.0 - 4.0 % Show Material materials with Aluminio of 3.0 - 4.0 % | Moderate Strength |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % | Moderate Strength |
Circonio | 3.5 - 4.5 % Show Material materials with Circonio of 3.5 - 4.5 % | Moderate Strength |
Cromo | 5.5 - 6.5 % Show Material materials with Cromo of 5.5 - 6.5 % | Moderate Strength |
Hidrógeno | 0.02 % Show Material materials with Hidrógeno of 0.02 % | Moderate Strength |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % | Moderate Strength |
Molibdeno | 3.5 - 4.5 % Show Material materials with Molibdeno of 3.5 - 4.5 % | Moderate Strength |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % | Moderate Strength |
Otro | 0.4 % Show Material materials with Otro of 0.4 % | Moderate Strength |
Oxígeno | 0.12 % Show Material materials with Oxígeno of 0.12 % | Moderate Strength |
Paladio | 0.04 - 0.08 % Show Material materials with Paladio of 0.04 - 0.08 % | Moderate Strength |
Titanio | 71.0 - 77.0 % Show Material materials with Titanio of 71.0 - 77.0 % | Moderate Strength |
Vanadio | 7.5 - 8.5 % Show Material materials with Vanadio of 7.5 - 8.5 % | Moderate Strength |