General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación | 23.0 °C | 14 % Show Material materials with Elongación of 14 % | |
Límite elástico | 23.0 °C | 1150 MPa Show Material materials with Límite elástico of 1150 MPa | |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 23.0 °C | 1210 MPa Show Material materials with Resistencia a la tracción of 1210 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Material materials with Calor específico of 450 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | |
Conductividad térmica | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Conductividad térmica of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.04 % Show Material materials with Azufre of 0 - 0.04 % |
Carbono | 0.38 - 0.43 % Show Material materials with Carbono of 0.38 - 0.43 % |
Cromo | 0.7 - 0.9 % Show Material materials with Cromo of 0.7 - 0.9 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 95.1 - 96.3 % Show Material materials with Hierro of 95.1 - 96.3 % |
Manganeso | 0.6 - 0.8 % Show Material materials with Manganeso of 0.6 - 0.8 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 1.7 - 2 % Show Material materials with Níquel of 1.7 - 2 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |