General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10 g/cm³ Show Material materials with Densidad of 10 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum |
Elongación | 23.0 °C | 12 % Show Material materials with Elongación of 12 % | |
Límite elástico | 23.0 °C | 360 MPa Show Material materials with Límite elástico of 360 MPa | |
Módulo de cizallamiento | 23.0 °C | 125 GPa Show Material materials with Módulo de cizallamiento of 125 GPa | Typical for Molybdenum |
Módulo elástico | 23.0 °C | 330 GPa Show Material materials with Módulo elástico of 330 GPa | |
Resistencia a la tracción | 23.0 °C | 590 MPa Show Material materials with Resistencia a la tracción of 590 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 250 J/(kg·K) Show Material materials with Calor específico of 250 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2E-5 1/K | |
Conductividad térmica | 23.0 °C | 117 - 431 W/(m·K) Show Material materials with Conductividad térmica of 117 - 431 W/(m·K) | Typical for Molybdenum |
Temperatura de fusión | 2610 °C Show Material materials with Temperatura de fusión of 2610 °C | Typical for Molybdenum |
Chemical properties
Property | Value |
---|---|
Carbono | 0.01 - 0.03 % Show Material materials with Carbono of 0.01 - 0.03 % |
Circonio | 0.06 - 0.12 % Show Material materials with Circonio of 0.06 - 0.12 % |
Hierro | 0 - 0.01 % Show Material materials with Hierro of 0 - 0.01 % |
Molibdeno | 99.3 - 99.5 % Show Material materials with Molibdeno of 99.3 - 99.5 % |
Nitrógeno | 0 - 2E-3 % Show Material materials with Nitrógeno of 0 - 2E-3 % |
Níquel | 0 - 2E-3 % Show Material materials with Níquel of 0 - 2E-3 % |
Oxígeno | 0 - 3E-3 % Show Material materials with Oxígeno of 0 - 3E-3 % |
Silicona | 0 - 0.01 % Show Material materials with Silicona of 0 - 0.01 % |
Titanio | 0.4 - 0.55 % Show Material materials with Titanio of 0.4 - 0.55 % |