General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación | 23.0 °C | 46 % Show Material materials with Elongación of 46 % | |
Límite elástico | 23.0 °C | 220 MPa Show Material materials with Límite elástico of 220 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | |
Resistencia a la tracción | 23.0 °C | 610 MPa Show Material materials with Resistencia a la tracción of 610 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Material materials with Calor específico of 450 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Boro | 1.5E-3 - 5E-3 % Show Material materials with Boro of 1.5E-3 - 5E-3 % |
Carbono | 0.04 - 0.1 % Show Material materials with Carbono of 0.04 - 0.1 % |
Cromo | 17 - 19 % Show Material materials with Cromo of 17 - 19 % |
Fósforo | 0 - 0.05 % Show Material materials with Fósforo of 0 - 0.05 % |
Hierro | 64 - 74 % Show Material materials with Hierro of 64 - 74 % |
Manganeso | 0 - 2 % Show Material materials with Manganeso of 0 - 2 % |
Nitrógeno | 0 - 0.1 % Show Material materials with Nitrógeno of 0 - 0.1 % |
Níquel | 9 - 13 % Show Material materials with Níquel of 9 - 13 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |
Titanio | 0 - 0.8 % Show Material materials with Titanio of 0 - 0.8 % |