General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 10 g/cm³ Show Material materials with Densidad of 10 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | Typical for Silver |
Elongación | 23.0 °C | 1.2 % Show Material materials with Elongación of 1.2 % | |
Módulo de cizallamiento | 23.0 °C | 30 GPa Show Material materials with Módulo de cizallamiento of 30 GPa | Typical for Silver |
Módulo elástico | 23.0 °C | 86 GPa Show Material materials with Módulo elástico of 86 GPa | |
Resistencia a la tracción | 23.0 °C | 520 MPa Show Material materials with Resistencia a la tracción of 520 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 250 J/(kg·K) Show Material materials with Calor específico of 250 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | |
Conductividad térmica | 23.0 °C | 417 - 428 W/(m·K) Show Material materials with Conductividad térmica of 417 - 428 W/(m·K) | Typical for Silver |
Temperatura de fusión | 780 °C Show Material materials with Temperatura de fusión of 780 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 5E-3 % Show Material materials with Aluminio of 0 - 5E-3 % |
Cadmio | 0 - 0.05 % Show Material materials with Cadmio of 0 - 0.05 % |
Cobre | 9 - 10.4 % Show Material materials with Cobre of 9 - 10.4 % |
Fósforo | 0 - 0.02 % Show Material materials with Fósforo of 0 - 0.02 % |
Hierro | 0 - 0.05 % Show Material materials with Hierro of 0 - 0.05 % |
Níquel | 0 - 0.01 % Show Material materials with Níquel of 0 - 0.01 % |
Otro | 0 - 0.06 % Show Material materials with Otro of 0 - 0.06 % |
Plata | 89.6 - 91 % Show Material materials with Plata of 89.6 - 91 % |
Plomo | 0 - 0.03 % Show Material materials with Plomo of 0 - 0.03 % |
Zinc | 0 - 0.06 % Show Material materials with Zinc of 0 - 0.06 % |