General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.26 - 8.8 g/cm³ Show Material materials with Densidad of 8.26 - 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 305 - 559 mm Show Material materials with Ancho of 305 - 559 mm |
Diámetro exterior | 9.5 - 76 mm Show Material materials with Diámetro exterior of 9.5 - 76 mm |
Espesor | 12.7 - 203.2 mm Show Material materials with Espesor of 12.7 - 203.2 mm |
Longitud | 610 - 3200 mm Show Material materials with Longitud of 610 - 3200 mm |
Wall thickness | 10-20% of outside diameter |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 37 - 45 [-] Show Material materials with Dureza Rockwell C of 37 - 45 [-] | |
Elongación | 23.0 °C | 1 - 75 % Show Material materials with Elongación of 1 - 75 % | for wire with 0.1mm diameter and more. |
Límite elástico | 23.0 °C | 630 MPa Show Material materials with Límite elástico of 630 MPa | |
Límite elástico Rp 0,2 | 23.0 °C | 130 - 1380 MPa Show Material materials with Límite elástico Rp 0,2 of 130 - 1380 MPa | |
Módulo de cizallamiento | 23.0 °C | 50 GPa Show Material materials with Módulo de cizallamiento of 50 GPa | |
Módulo elástico | 23.0 °C | 130 - 131 GPa Show Material materials with Módulo elástico of 130 - 131 GPa | |
Resistencia a la tracción | 23.0 °C | 410 - 1550 MPa Show Material materials with Resistencia a la tracción of 410 - 1550 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 360 J/(kg·K) Show Material materials with Calor específico of 360 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 - 1.8E-5 1/K |
Conductividad térmica | 23.0 °C | 84 - 130 W/(m·K) Show Material materials with Conductividad térmica of 84 - 130 W/(m·K) |
Temperatura de fusión | 870 °C Show Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 7.9E-8 - 7.8E-6 Ω·m Show Material materials with Resistividad eléctrica of 7.9E-8 - 7.8E-6 Ω·m |
Specific Electrical conductivity | 22 - 30 % IACS Show Material materials with Specific Electrical conductivity of 22 - 30 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 1.8 - 2 % Show Material materials with Berilio of 1.8 - 2 % | |
Cobalto | 0.2 - 0.3 % Show Material materials with Cobalto of 0.2 - 0.3 % | min. Nickel + Cobalt,max. |
Cobre | 96.1 - 98 % Show Material materials with Cobre of 96.1 - 98 % | Balance |
Hierro | 0 - 0.6 % Show Material materials with Hierro of 0 - 0.6 % | max., Nickel + Cobalt + Iron,max. Nickel + Cobalt + Iron |
Níquel | 0.2 - 0.6 % Show Material materials with Níquel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Otro | 0 - 0.6 % Show Material materials with Otro of 0 - 0.6 % | max., Co+Ni+Fe |
Plomo | 0.2 - 0.6 % Show Material materials with Plomo of 0.2 - 0.6 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include wear plates and other galling resistant components.,Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts,Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration.,EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good machinability |