General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.83 - 8.9 g/cm³ Show Material materials with Densidad of 8.83 - 8.9 g/cm³ |
Medidas
Property | Value | Comment | |
---|---|---|---|
Ancho | 305 - 559 mm Show Material materials with Ancho of 305 - 559 mm | ||
Diámetro | 1.27 - 12.7 mm Show Material materials with Diámetro of 1.27 - 12.7 mm | ||
Diámetro exterior | 0.76 - 76 mm Show Material materials with Diámetro exterior of 0.76 - 76 mm | Rod | |
Espesor | 0.76 - 76 mm Show Material materials with Espesor of 0.76 - 76 mm | Bar | |
Longitud | 610 - 91000 mm Show Material materials with Longitud of 610 - 91000 mm | max. Rod and Bar | |
Wall thickness | Typically 10 to 20% of OD |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 - 20 % Show Material materials with Elongación of 2 - 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 340 - 550 MPa Show Material materials with Límite elástico Rp 0,2 of 340 - 550 MPa |
Módulo elástico | 23.0 °C | 120 - 138 GPa Show Material materials with Módulo elástico of 120 - 138 GPa |
Resistencia a la tracción | 23.0 °C | 440 - 590 MPa Show Material materials with Resistencia a la tracción of 440 - 590 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 390 J/(kg·K) Show Material materials with Calor específico of 390 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.76E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 210 - 240 W/(m·K) Show Material materials with Conductividad térmica of 210 - 240 W/(m·K) |
Temperatura de fusión | 1030 - 1040 °C Show Material materials with Temperatura de fusión of 1030 - 1040 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Material materials with Resistividad eléctrica of 2.9E-6 - 3.8E-6 Ω·m |
Specific Electrical conductivity | 45 - 60 % IACS Show Material materials with Specific Electrical conductivity of 45 - 60 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 0.2 - 0.6 % Show Material materials with Berilio of 0.2 - 0.6 % | |
Cobalto | 0 - 0.3 % Show Material materials with Cobalto of 0 - 0.3 % | |
Cobre | 95.9 - 98.4 % Show Material materials with Cobre of 95.9 - 98.4 % | Balance |
Hierro | 0 - 0.1 % Show Material materials with Hierro of 0 - 0.1 % | |
Níquel | 1.4 - 2.2 % Show Material materials with Níquel of 1.4 - 2.2 % | |
Otro | 0 - 0.5 % Show Material materials with Otro of 0 - 0.5 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding.,Typical applications include dies casting plunger tips and dies for steel extrusion.,Typical applications include heat exchanger tubing and resistance welding components.,Typical applications include coil springs and formed wire contacts. |