General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.41 - 8.8 g/cm³ Show Material materials with Densidad of 8.41 - 8.8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 305 - 559 mm Show Material materials with Ancho of 305 - 559 mm | |
Diámetro | 0.76 - 76 mm Show Material materials with Diámetro of 0.76 - 76 mm | |
Diámetro exterior | 9.5 - 76 mm Show Material materials with Diámetro exterior of 9.5 - 76 mm | |
Espesor | 4.8 - 76 mm Show Material materials with Espesor of 4.8 - 76 mm | |
Longitud | 610 - 91000 mm Show Material materials with Longitud of 610 - 91000 mm | max. |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 3.8 - 30 % Show Material materials with Elongación of 3.8 - 30 % |
Límite elástico | 23.0 °C | 1010 MPa Show Material materials with Límite elástico of 1010 MPa |
Límite elástico Rp 0,2 | 23.0 °C | 520 - 720 MPa Show Material materials with Límite elástico Rp 0,2 of 520 - 720 MPa |
Módulo elástico | 23.0 °C | 120 - 131 GPa Show Material materials with Módulo elástico of 120 - 131 GPa |
Resistencia a la tracción | 23.0 °C | 590 - 1180 MPa Show Material materials with Resistencia a la tracción of 590 - 1180 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 410 J/(kg·K) Show Material materials with Calor específico of 410 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.75E-5 1/K |
Conductividad térmica | 23.0 °C | 105 - 110 W/(m·K) Show Material materials with Conductividad térmica of 105 - 110 W/(m·K) |
Temperatura de fusión | 870 °C Show Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.8E-6 - 6.9E-6 Ω·m Show Material materials with Resistividad eléctrica of 5.8E-6 - 6.9E-6 Ω·m |
Specific Electrical conductivity | 25 - 30 % IACS Show Material materials with Specific Electrical conductivity of 25 - 30 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 1.6 - 1.85 % Show Material materials with Berilio of 1.6 - 1.85 % | |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % | min. Nickel + Cobalt |
Cobre | 96.3 - 98.2 % Show Material materials with Cobre of 96.3 - 98.2 % | Balance |
Hierro | 0 - 0.6 % Show Material materials with Hierro of 0 - 0.6 % | max., Nickel + Cobalt + Iron |
Níquel | 0.2 - 0.6 % Show Material materials with Níquel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Otro | 0 - 0.5 % Show Material materials with Otro of 0 - 0.5 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include bushings, bearings and resistance welding components.,Alloy 165 tube is used in crucial telecommunications applications including undersea instrument housings and repeater housings.,Typical applications include wear plates and resistance welding components. |